ISOLATOR FOR GALVANIC CORROSION IN CARBON FIBER

Isolator

June 19, 2017

Typically a concern when mating different metals, galvanic corrosion can affect carbon fiber composite-to-aluminum couplings. Vesconite, the advanced marine polymer, makes the ideal electrical isolator when working with potentially problematic dissimilar materials.

Perfect for high load applications, Vesconite has particularly high dimensional stability and compression strength, unlike nylon that softens when wet and easily deforms. It machines to +/-0.001″, so intricate parts can easily be fabricated—something that’s important when fitting-in custom-built components.

When used as a bearing, such as between a metal pivot pin and a carbon fiber-reinforced canting keel or downrigger pole, it’s the perfect material. Added to its unique anti-galvanic corrosion properties, Vesconite is self-lubricating, and offers low friction and superior wear-resistance—10 times that of bronze.

Vesconite is available in the US as finished parts, or as hollow bar, solid rod and plate stock in a wide range of dimensions and thicknesses. It bears type approval certifications from such agencies as ABS, Bureau Veritas and Det Norske Veritas. It is accredited to ISO 9001. www.vesconite.com.

Related Posts





Vote for Dorothy, BC’s Iconic Sailing Yacht, in the Classic Boat Awards 2024

CMRA

You are invited to support an historic, recently restored and refitted BC sailboat, Dorothy, by voting for her in a contest, the Classic Boat Awards 2024, run by the UK’s prestigious Classic Boat Magazine. The Maritime Museum of BC (MMBC), owner of this sleek, wooden vessel built in 1897, believes she’s the oldest sailboat in Canada. As she isn’t the only classic yacht in the running, you’re urged to go online and vote for her in the category of Restored Sailing Vessel under 40ft.

Read More




Need to Catch up on News This Week?

Every Tuesday we publish a fresh Digest with informative articles pertaining to the Canadian boating and marine industry. Stay up to date with the latest products, research and industry developments.

Missed an Issue of Boating Industry Canada News Week? If you’re looking for a specific issue, or simply want to catch up on previous issues, check out our Boating Industry Canada News Week Archives.

Not signed up for News Week? Subscribe here.



Even more BALIs at BALI

CATANA GROUP launches its 14th BALI CATAMARANS model, the BALI 5.8, for the brand’s 10th anniversary! Always bigger, always more powerful, always more… BALI!

This time, the new BALI 5.8 is completing the range from the top down.

Read More


Water heater offers dynamic heat source choices

Hubbell-Marine Stainless steel outlet covers
Hubbell-Marine Stainless steel outlet covers

After a long day on the water, having ample supplies of hot water for multiple showers and meal preparation is a welcome luxury. The 1700 Series Marine Water Heater from Raritan Engineering was created specifically for marine use. With a proven long-life design, it’s available with a 115V AC or 240V AC heating element, and the option to include an innovative heat exchanger that uses the vessel’s hot engine coolant.

Read More